worldinoutRegisterLogin | Set Homepage | Save desktop | Mobile | Qr code
Member
Guangzhou Pinbang Building Material Industrial Company
Ceramic Wall Tile Adhesive;Ceramic Floor Tile Adhesive;Marble Tile Adhesive
 
Your current location:Home » Sell » High Strength Interior Cement Wall Putty Cement Based Mortar

High Strength Interior Cement Wall Putty Cement Based Mortar

Click image to view full size image
Title: High Strength Interior Cement Wall Putty Cement Based Mortar 
Brand: -
Model: -
Unit price: Negotiable
MOQ: -0 -
Quantity: Negotiable
Delivery date: Since the payment date Days delivery

Contact: Joe Yuan (Ms.)    
Mobile:
Telephone:

  Inquiry
Details

 

High Strength Interior Cement Wall Putty Cement based Mortar

 

 

Product Description:

 

1. PB-08 Retread Skim Coat is high-strength, cement-based mortar with fine-grained selected aggregates, special admixtures and synthetic polymers in water dispersion.
2. This product is specially developed for the high-level external wall putty in order to apply the high-level wall putty market, provides a flat base surface and has strong adhesive force to the coating
 

 

Features and Benefits:


1, Crackless application.
2, Mixes easily with potable water.
3, High-ductility smoothing and leveling layer on concrete repaired.
4, High bonding strength.
5, Impermeable to water and aggressive gases present in the atmosphere.
 

 

Operation Process:

 

1, The ratio: powder: water: additive: 8: (2~2.8): 1.

2, The substrate surface should be firm, dry and clean, no grease, no wax, and other loose materials.

3, If the wall is too dry, wet the wall before operation till there is no obvious water on the surface.

4, Pouring the water into the stirring barrel, adding the powder slowly, stirring them into particle paste with no powder no deposition, using inserting tools to batch, after 4~6h of the first insert can make the second time, polishing the lacquer putty layer, control the thickness between 0.8~1.5mm.

5, During the insert process, pay attention to the even and flaws.

6, When finishing the putty, according to the weather to polish within 1~2 days.

7, After 7 days of the inserting putty, can paint other coatings, for the alkali resisting primer the time can shorten.

 

 

Dosage:


1.0~1.5 kg/m² per mm of thickness.
Few dosages for the even surface.

 

 

Technical Reference:

 

Shrinkage(%)

≤0.5MPa

Tensile strength resistance to temperature

≥1.2MPa

Compression and shear bond strength

≥1.5MPa